Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 55000 cP | 55000 cP | |
Momentive Performance Materials TSE3221 Flowable, Heat Cured One Component Silicone Adhesive TSE 3221 is a one-component, flowable, heat curing adhesive which is translucent in color and offers primerless adhesion to a wide variety of substrates. This product requires an elevated temperatur.. |
|||
Viscosity | 55000 cP | 55000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Viscosity | 55000 cP | 55000 cP | |
Shin-Etsu Silicones KE-347T Silicone, RTV Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 55000 - 110000 cP | 55000 - 110000 cP | Part A |
Master Bond EP30HT-LO NASA Low Outgassing, Optically Clear Coating Description: Master Bond EP30HT-LO is a moderate viscosity, two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio.. |
|||
Viscosity | 55000 - 110000 cP | 55000 - 110000 cP | Part A |
Master Bond EP65HT Fast Setting Epoxy Resists High Temperatures Description: Master Bond EP65HT represents a highly innovative advance in epoxy technology in that it features the unusual combination of very fast cures and high temperature resistance. While typic.. |
|||
Viscosity | 55000 - 110000 cP | 55000 - 110000 cP | Part A |
Master Bond EP30M4 Chemically Resistant Two Component Epoxy System Master Bond Polymer System EP30M4 is a two component epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weight. EP30M4 resi.. |
|||
Viscosity | 55000 cP | 55000 cP | mixing, dynamic |
Dow Corning SILASTIC® E RTV SILICONE RUBBER KIT High strength silicone mold making rubber recommended for use with polyester or plaster and can be used with rigid and foam polyurethanes and epoxies.Information provided by Dow Corning |
|||
Viscosity | 55000 cP | 55000 cP | mixing, dynamic |
Dow Corning SILASTIC® T-2 RTV SILICONE TRANSLUCENT BASE & CURING AGENT Translucent, high strength silicone mold making rubber suited for prototype design and production tooling. Silastic T-2 is recommended for use with rigid polyurethane and can be used with polyesters.. |
|||
Viscosity | 55000 - 90000 cP @Temperature 23.0 °C |
55000 - 90000 cP @Temperature 73.4 °F |
1 rpm |
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |
|||
Viscosity | 55000 cP | 55000 cP | Base |
ACC QM 262F QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 262F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin.. |
|||
Viscosity | 55000 cP | 55000 cP | |
ACC QSil 60 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting QSil 60 is a red, high temperature, self-leveling, two-component, silicone material primarily used for potting applications. The two applicable catalysts are 0.5% DBT by weight and 10% Deep Section .. |