Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5.0 cP | 5.0 cP | |
Ritelok ECS Ethyl CA Adhesive Cyanoacrylate. Designed to penetrate by capillary action between pre-assembled components. High Strength, Low viscosity, Penetrating action |
|||
Viscosity | 5.0 cP | 5.0 cP | |
ND Industries 623 Heptane-Acetone SuperGlue accelerator Fast Acting SuperGlue accelerator, general purpose for porous surfaces or large gaps. Non-ozone depleting but flammable solvent |
|||
Viscosity | 5.0 cP | 5.0 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120 LOW ODER advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's p.. |
|||
Viscosity | >= 5.0 cP | >= 5.0 cP | ASTM D2196 |
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6101 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6201 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6001 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6002 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6801 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6802 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6901 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Viscosity | 5.0 - 20 cP | 5.0 - 20 cP | As Supplied |
Heraeus Cleviosâ„¢ P Jet HC Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet HC is an antistatic material based on PE.. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
As Supplied |
Heraeus Cleviosâ„¢ P Jet HC V2 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet HC V2 is an antistatic material based on.. |
|||
Viscosity | 5.0 - 25 cP | 5.0 - 25 cP | |
Huntsman Araldite DY 023 Reactive Diluent Weight per Epoxide (EEW, g/eq) 167 to 182. Max color is 1.Comments/Applications: Cresyl glycidyl ether - monofunctional epoxy. Less volatile and better resistance to water, but less efficient visc.. |
|||
Viscosity | 5.0 - 15 cP @Temperature 20.0 °C |
5.0 - 15 cP @Temperature 68.0 °F |
2%, Hoppler |
Mikro-Technik DT R Carboxymethylcellulose (CMC) Purified GradeComments: All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E). Reduced active contents down to 50 % are available. Special conce.. |
|||
Viscosity | 5.0 - 20 cP | 5.0 - 20 cP | As Supplied |
Heraeus Cleviosâ„¢ P Jet 700 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet 700 is an antistatic material based on P.. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
|
Heraeus Cleviosâ„¢ P Jet N Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PT2 is an antistatic material based on PEDOT:P.. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
As Supplied |
Heraeus Cleviosâ„¢ P Jet N V2 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet N V2 is an antistatic material based on .. |
|||
Viscosity | 5.0 - 6.0 cP @Temperature 20.0 °C |
5.0 - 6.0 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 51-05 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Loctite® 408 Low odor/low bloom Alkoxy Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 5.0 - 15 cP | 5.0 - 15 cP | ASTM D445 |
ExxonMobil Jayflex™ MB10 Plasticizer Availability: AmericasCAS Number: 131298-44-7EINECS Number: 421-090-1Information provided by ExxonMobil |
|||
Viscosity | 5.0 - 15 cP | 5.0 - 15 cP | ASTM D445 |
ExxonMobil Jayflex™ MB10 Plasticizer (European Grade) Availability: Europe, Middle East & AfricaCAS Number: 131298-44-7EINECS Number: 421-090-1Information provided by ExxonMobil |
|||
Viscosity | 5.0 cP @Temperature 43.0 °C |
5.0 cP @Temperature 109 °F |
|
Dow ISONATE™ 125M Pure MDI ISONATE™ 125M is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This di-functional product is a key ingredient in preparing prepolymers f.. |
|||
Viscosity | 5.0 cP @Temperature 43.0 °C |
5.0 cP @Temperature 109 °F |
|
Dow ISONATE™ 125MDR Pure MDI ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers .. |
|||
Viscosity | <= 5.0 cP | <= 5.0 cP | |
3M Scotch-Weld™ AC78 Instant Adhesive Primer 3M™ Scotch-Weld™ Instant Adhesive Primer AC78 helps to bind elastomeric materials including silicone.Information provided by 3M |
|||
Viscosity | 5.0 - 30 cP | 5.0 - 30 cP | @ 275 |
ACC 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion 1KSP is a silicone modified polyurea dispersion “Powered by ReactAmine® Technology” designed for a wide range of rigid and flexible substrates such as wood, metal, vinyl, concrete and other plast.. |
|||
Viscosity | 5.0 cP @Temperature 25.0 °C |
5.0 cP @Temperature 77.0 °F |
|
Parker Chomerics CHO-SHIELD® 1085 Silicone Adhesive Primer Air-drying liquid coatings used to improve the adhesion of Chomerics CHO-BOND conductive silicone elastomers to metal and other non-silicone substrates. The primers are moisture reactive and clear i.. |