Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 400000 cP @Shear Rate 190 1/s, Temperature 230 °C |
400000 cP @Shear Rate 190 1/s, Temperature 446 °F |
|
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Viscosity | 400000 cP | 400000 cP | melt; SABIC Method |
SABIC Innovative Plastics Valox® EF4530 PBT (Asia Pacific) Easy flow, 30% glass-reinforced, PBTP resin. Flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Viscosity | 400000 cP | 400000 cP | Melt Viscosity; SABIC Method |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Viscosity | 400000 cP | 400000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 400000 cP | 400000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 400000 cP | 400000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE2090-30AB Elastomer KE-2090-30 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 400000 cP @Temperature 25.0 °C |
400000 cP @Temperature 77.0 °F |
Dynamic |
Struktol VP 3695 Elastomer modified epoxy prepolymer Applications: STRUKTOL POLYDIS 3695 is used where conventional epoxy systems are unable to satisfy the demands of for example contact adhesion or peel strength. Improvements in impact strength, flex.. |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F130-E1 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F132-E1 PA6 Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F132-E2 PA6 High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F136 PA6 Very High Viscosity, Film Extrusion |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F136-C PA6 Film Extrusion, Very High Viscosity, Lubricated |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Viscosity | 400000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
400000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Viscosity | 400000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
400000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 400000 cP | 400000 cP | Mixed |
Armstrong A-1/V Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Viscosity | >= 400000 cP | >= 400000 cP | 0.5 rpm, uncured |
Atom Adhesives AA-BOND G298 Epoxy Adhesive AA-BOND G298 is a two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Appearance: Resin: Brown, Hardener: Dark Bro.. |
|||
Viscosity | 400000 - 800000 cP @Shear Rate 100 1/s, Temperature 232 °C |
400000 - 800000 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Viscosity | 400000 - 800000 cP @Shear Rate 100 1/s, Temperature 232 °C |
400000 - 800000 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Viscosity | 400000 cP | 400000 cP | Mixed |
Armstrong A-1/E Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Viscosity | 400000 cP @Shear Rate 300 1/s, Temperature 190 °C |
400000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 4660 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Viscosity | 400000 cP @Temperature 400 °C |
400000 cP @Temperature 752 °F |
Melt; ISO 11443 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Viscosity | 400000 cP | 400000 cP | Mixed; TM R050-12 |
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |