Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4.0 - 750 cP | 4.0 - 750 cP | |
Kazanorgsintez NMPE-1 Low-Molecular Polyethylene Low-molecular polyethylene of high pressure polyethylene production. Application: Designed for use in the rubber industry, building industry, and other fields. Can also be used as component parts.. |
|||
Viscosity | 4.0 - 20 cP | 4.0 - 20 cP | As Supplied |
Heraeus Cleviosâ„¢ P Jet (OLED) Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet (OLED) is an antistatic material based o.. |
|||
Viscosity | 4.0 cP @Temperature 25.0 °C |
4.0 cP @Temperature 77.0 °F |
|
LyondellBasell DPM Dipropylene glycol methyl ether Information provided by Lyondell. |
|||
Viscosity | 4.0 - 6.0 cP | 4.0 - 6.0 cP | 20% aq. Sol.; L170 |
Solvay GLOKILL® PQ Surfactant Description: Cationic polymer based on quaternary ammonium.Identification: POLYQUATERNARY AMMONIUM CHLORIDE AQUEOUS SOLUTIONAvailable in: Asia Pacific, Europe, Latin America and North AmericaStabili.. |
|||
Viscosity | 4.0 - 8.0 cP | 4.0 - 8.0 cP | 20% aq. Sol.; L170 |
Solvay GLOKILL® PQ60 Surfactant Description: Algicide and biocide for swimming poolIdentification: POLYQUARTERNARY AMMONIUM CHLORIDE, AQUEOUS SOLUTIONCAS: 25988 – 97 – 0Available in: EuropeFunction: Algaecide for use in .. |
|||
Viscosity | 4.0 - 5.0 cP @Temperature 20.0 °C |
4.0 - 5.0 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 51-04 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 4.0 - 5.0 cP @Temperature 20.0 °C |
4.0 - 5.0 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-04 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 4.0 - 8.0 cP | 4.0 - 8.0 cP | |
Daikin NEOFLON ND-2 FEP Dispersion, Milky White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Viscosity | 4.0 cP @Temperature 25.0 °C |
4.0 cP @Temperature 77.0 °F |
|
LyondellBasell PTB Propylene glycol tertiary butyl ether Information provided by Lyondell. |