Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3500 cP @Temperature 190 °C |
3500 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 2535 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Low softening point, excellent tack, excellent flexibility, and long open timeApplications: Component of hot mel.. |
|||
Viscosity | 3500 - 5000 cP | 3500 - 5000 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The produ.. |
|||
Viscosity | 3500 cP @Temperature 25.0 °C |
3500 cP @Temperature 77.0 °F |
Uncured |
Permabond HM163 Anaerobic Retainer Permabond® HM163 is a medium viscosity, thixotropic anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It has been specifically formulated to provide a .. |
|||
Viscosity | 3500 cP | 3500 cP | Part A |
Resinlab® EP324E Clear Two Part Epoxy Casting Resin Resinlab™ EP 324E Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wettin.. |
|||
Viscosity | 3500 cP @Temperature 190 °C |
3500 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 3535 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Excellent low temperature flexibilityApplications: Component of modified bitumen roofing systemsOther Proper.. |
|||
Viscosity | 3500 - 10000 cP | 3500 - 10000 cP | |
Huntsman Araldite GZ 9625 W-90 Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 230 to 280. Max color is 3.Comments/Applications: Bisphenol A epoxy resin cut in n-Butanol. High solids coatings for maintenance and marine applications.Data provide.. |
|||
Viscosity | 3500 - 4000 cP | 3500 - 4000 cP | as supplied |
Industrial Nanotech Nansulateâ„¢ PT Translucent Insulation Coating Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general insulation use for pipes, tanks, and metallic surfaces.NANSULATEâ„¢.. |
|||
Viscosity | 3500 cP | 3500 cP | Mixed Viscosity |
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear Information provided by ITW Devcon |
|||
Viscosity | 3500 - 7000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3500 - 7000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2030812D3 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 60/40. Applications in medical diagnostics, environmentalScreen Printing Equipment: semi-automatic, manualScreen Types: polye.. |
|||
Viscosity | 3500 - 7000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3500 - 7000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2051014P10 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. Applications in medical diagnostics, environmentalScreen Printing Equipment: semi-automatic, manualScreen Types: polye.. |
|||
Viscosity | 3500 - 7000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3500 - 7000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080110D2 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 70/30. This is has been designed for fine line printing.Screen Printing Equipment: semi-automatic, manualScreen Types: polye.. |
|||
Viscosity | 3500 - 7000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3500 - 7000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080409D2 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 85/15. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste.. |
|||
Viscosity | 3500 - 5000 cP | 3500 - 5000 cP | |
Lucite International Colacryl ® 1204 Acrylic Solution Resin Butyl Methacrylate polymers are more flexible and softer than Methyl Methacrylate types. The polymers are compatible with nitrocellulose, chlorinated rubber, some phenolics and maleics. Butyl methac.. |
|||
Viscosity | 3500 - 5500 cP | 3500 - 5500 cP | ASTM D803 |
SK Chemicals SKYTHANE® U1731C Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 3500 cP @Temperature 25.0 °C |
3500 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2170 Flexible Plastic Bonder TRA-BOND 2170 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermoplas.. |
|||
Viscosity | 3500 cP | 3500 cP | Part A at 20 RPM |
Loctite® 3292 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Viscosity | 3500 - 5000 cP @Temperature 23.0 °C |
3500 - 5000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® 323LP Epoxy Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology |
|||
Viscosity | 3500 - 6000 cP @Temperature 23.0 °C |
3500 - 6000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy Material Description: A slightly longer pot life version of EPO-TEK®353ND designed for high temperature, optical and structural applications inside the semiconductor, hybrid, electronic, fiber opti.. |
|||
Viscosity | 3500 cP @Temperature 25.0 °C |
3500 cP @Temperature 77.0 °F |
|
Esstech X-726-0000 PEG 400 Extended Urethane Dimethacrylate, C54H98N4O21 Our extended UDMA is commonly used in light cure systems. Its PEG 400 portion creates a more flexible polymer upon curing. Adding this product has been shown to increase the fracture toughness of ur.. |
|||
Viscosity | 3500 cP | 3500 cP | Dynamic |
Dow Corning XIAMETER® PMCPOFX-8630 Fluid Is chemically equivalent to DOW CORNING® 2-8630 POLYMER. 100% active, amino-functional silicone polymer.Information provided by Dow Corning |
|||
Viscosity | 3500 cP | 3500 cP | |
Dymax 928 Coil Terminating, Tamper proofing and Structural Electronic Bonder High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 928 Coil Terminating, Tamper proofing and Structural Electronic BonderHigh strength, excellent bridge bonding capabi.. |
|||
Viscosity | 3500 - 6500 cP | 3500 - 6500 cP | |
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Viscosity | >= 3500 cP | >= 3500 cP | Base |
3M Scotch-Weld™ DP807 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Viscosity | >= 3500 cP | >= 3500 cP | Base |
3M Scotch-Weld™ DP825 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Viscosity | 3500 - 6000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3500 - 6000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2010309P3 Platinum Paste This product has been designed as a platinum paste suitable for high temperature firing applications on to electro-ceramic substrates such as NTC. It is capable of withstanding repeated firing at h.. |