Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 35 - 60 cP | 35 - 60 cP | |
ND Industries 306 Surface Insensitive Instant Superglue Low viscosity for difficult to bond rubber compounds |
|||
Viscosity | 35 - 60 cP | 35 - 60 cP | 3 |
ND Industries SuperGlue Ethyl 395 General DescriptionA low viscosity ethyl-based cyanoacrylate that exhibits fast cure speeds on a wide range of common materials such as metals, rubbers, and plastics.Typical Usesloudspeaker componen.. |
|||
Viscosity | 35 - 45 cP | 35 - 45 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 120 (40 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 35 - 45 cP | 35 - 45 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 120 LOW ODOR/LOW BLOOM (40 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120 LOW ODER advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's p.. |
|||
Viscosity | 35 - 45 cP | 35 - 45 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 120SI Surface Insensitive (40 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Viscosity | 35 cP | 35 cP | 5% Toluene Solution; ASTM D445 |
LG Chemical LG-428N Styrene-Butadiene-Styrene Description: Radial structure, Non-Oil Extended Grade Thermoplastic ElastomerApplications: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS: 9003-55-8Information provided by LG Chem.. |
|||
Viscosity | 35 - 100 cP | 35 - 100 cP | ASTM D445 |
IRPC Polimaxx Polene PE220NSC Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Viscosity | 35 cP @Temperature 200 °C |
35 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3230 Polyester, Flake Adhesive agent, Resin modifierUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binde.. |
|||
Viscosity | 35 - 60 cP @Temperature 25.0 °C |
35 - 60 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 11 Heat Cure Catalyst Emerson & Cuming 11 Eccobond® Heat Cure CatalystGeneral purpose, low viscosity, elevated temperature curing. Long working life. Yields cured coatings with excellent chemical resistance. Subject to .. |
|||
Viscosity | 35 cP | 35 cP | (mixed) |
Loctite® Shadowcure™ 394 Acrylic/urethane UV Coating Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Locti.. |
|||
Viscosity | 35 cP @Temperature 25.0 °C |
35 cP @Temperature 77.0 °F |
Value represents initial mixed viscosity of components. |
Cytec Conathane® CC-1155-35 (Conap) Polyurethane Two-component Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Viscosity | 35 cP | 35 cP | |
BASF Lupranate® 230 Isocyanate Description: Lupranate® 230 Isocyanate is a low viscosity derivative of both pure-MDI and polymeric-MDI. With a functionality of approximately 2.2, this isocyanate can be formulated into applicatio.. |
|||
Viscosity | 35 cP | 35 cP | |
BASF Lupranate® 245 Isocyanate Description: Lupranate® 245 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric MDI) containing a very high amount of monomeric diphenylmethane diisocyanate (pure MDI)In.. |
|||
Viscosity | 35 cP | 35 cP | B Component; ASTM D1824 |
Aptek 2100-A7C/B Low modulus urethane staking compound APTEK 2100-A7C/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Althoug.. |
|||
Viscosity | 35 cP | 35 cP | |
Aremco Ceramabind™ 644-S High Temperature Inorganic Binder A colloidal silica aqueous solution which produces high adhesive strength. Ideal for blending with all types of granular and fibrous ceramics. Excellent resistance to temperature, moisture and mecha.. |