Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 30000 cP | 30000 cP | Mixed; TM R050-12 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Viscosity | 30000 cP @Temperature 25.0 °C |
30000 cP @Temperature 77.0 °F |
|
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po.. |
|||
Viscosity | 30000 cP @Temperature 25.0 °C |
30000 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Viscosity | 30000 cP | 30000 cP | |
Momentive Performance Materials RTV560 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, Red RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Viscosity | 30000 cP | 30000 cP | Before Curing |
Silikony Polskie Gumosil WW Silicone Rubber Flexible with good tearing resistance |
|||
Viscosity | 30000 - 65000 cP | 30000 - 65000 cP | mixed compound; thixotropic |
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun.. |
|||
Viscosity | 30000 - 40000 cP | 30000 - 40000 cP | |
Master Bond MasterSil 709 One Part Silicone Meets MIL Spec Description: MasterSil 709 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This unique product meets the MIL.. |
|||
Viscosity | 30000 cP @Temperature 25.0 °C |
30000 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 2979LV Microelectronic Conductive Epoxy Adhesive TRA-DUCT 2979LV is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid.. |
|||
Viscosity | 30000 cP | 30000 cP | Part A at 20 RPM |
Loctite® 3273 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Viscosity | 30000 cP | 30000 cP | Mixed - high; Resin - nonsag paste; Hardener - 30,000 cP |
Loctite® Durabond® E-20NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Viscosity | 30000 cP | 30000 cP | Dynamic |
Dow Corning 7-3118 EBAP Hip Emulsion A concentrated emulsion of dimethicone crosspolymer in cyclopentasiloxane and dimethicone that is designed to facilitate the rapid development of skin care formulations which contain these emollient.. |
|||
Viscosity | 30000 cP @Temperature 190 °C |
30000 cP @Temperature 374 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1533E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 30000 cP | 30000 cP | |
Epoxyset Epoxiohm EO-21 Electrically Conductive Epoxy Adhesive EO-21 is a two part, silver filled high electrical conductivity epoxy adhesive. It is designed to cure at room temperature or rapidly at elevated temperature and exhibits very excellent adhesion and.. |
|||
Viscosity | 30000 - 35000 cP | 30000 - 35000 cP | |
Epoxyset Epoxiohm EO-38M-3 Electrically Conductive Epoxy Adhesive EO-38M-3 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management appl.. |
|||
Viscosity | 30000 cP | 30000 cP | |
Dymax 3073 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | 30000 cP | 30000 cP | Thixotropic Gel |
Dymax 9-20524 Voil Coil Assembly Disk Drive Adhesive Disk Drive AdhesivesLow Outgassing Multi-Cure® Memory Saver Disk Drive AdhesivesDescriptionDymax offers a range of advanced formula epoxy and acrylic adhesives for disk drive assembly. UV cures in .. |
|||
Viscosity | 30000 cP | 30000 cP | Thixotropic Gel |
Dymax EMAX 10002 Voil Coil Assembly Disk Drive Adhesive Disk Drive AdhesivesLow Outgassing Multi-Cure® Memory Saver Disk Drive AdhesivesDescriptionDymax offers a range of advanced formula epoxy and acrylic adhesives for disk drive assembly. UV cures in .. |
|||
Viscosity | 30000 cP | 30000 cP | |
ACC MM239 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: ceramic/polyester/PU/epoxy a.. |
|||
Viscosity | 30000 cP | 30000 cP | catalyzed with QM 245B |
ACC QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material QM 245 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Viscosity | 30000 cP | 30000 cP | catalyzed with QM CAT PURPLE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Viscosity | 30000 cP | 30000 cP | catalyzed with QM CAT RED 3 |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Viscosity | 30000 cP | 30000 cP | A Component; ASTM D1824 |
Aptek 2201-A/B Fast set urethane adhesive APTEK 2201-A/B is a two component, dark gray, urethane adhesive system displaying excellent adhesion to various plastic, wood, ceramic, and metal substrates. APTEK 2201-A/B is capable of achieving f.. |
|||
Viscosity | 30000 - 40000 cP | 30000 - 40000 cP | |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 30000 cP | 30000 cP | |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Viscosity | 30000 cP | 30000 cP | Mixed; TM R050-12 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Viscosity | 30000 - 100000 cP | 30000 - 100000 cP | Thixotropic |
Loctite® 574 Semi-rigid Cure Anaerobic Sealant Anaerobic GasketingLoctite® 574 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Fast curing, large gaps |
|||
Viscosity | 30000 cP | 30000 cP | Mixed; TM R050-12 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |