Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2600 - 3200 cP | 2600 - 3200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-626H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Viscosity | 2600 - 3200 cP | 2600 - 3200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-632H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 2600 - 3200 cP | 2600 - 3200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-690H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations.. |
|||
Viscosity | 2600 cP | 2600 cP | |
Loctite® 246 High Temperature/Medium Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |