Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2100 - 3600 cP | 2100 - 3600 cP | |
Huntsman Araldite GY 502 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 222 to 238. Max color is 3.Comments/Applications: GY 6010 modified with dibutyl phthalate - a non-reactive diluent. Increases resiliency of cured product; suitable f.. |
|||
Viscosity | 2100 - 2500 cP | 2100 - 2500 cP | |
Huntsman Araldite GY 9613 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 188 to 197. Max color is 1.Comments/Applications: GY 2600 modified with DY 025 (Epoxide 8). Very light color. High solids and solvent free coatings and floorings.Da.. |
|||
Viscosity | 2100 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
2100 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors This material has a high viscosity, it is a water based acrylic pressure sensitive screen printable adhesive. It can be used in many different diagnostic applications such as test cards, assays and.. |
|||
Viscosity | 2100 cP @Temperature 25.0 °C |
2100 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 526M04 Color Keyed High Temperature Epoxy Adhesive TRA-BOND 526M04 is a low viscosity, high-temperature, two-part epoxy formulation with a long working life. TRA-BOND 526M04 exhibits excellent wicking, and develops strong, tough mechanically stable .. |
|||
Viscosity | 2100 cP @Temperature 25.0 °C |
2100 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond F253M Color Keyed High Temperature Epoxy Adhesive TRA-BOND F253M is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status. The unmixed components are light yellow; the mix.. |
|||
Viscosity | 2100 cP @Temperature 25.0 °C |
2100 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Cast 3012 Clear Epoxy Casting Compound TRA-CAST 3012 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties good clarity, long pot life,.. |
|||
Viscosity | 2100 - 2500 cP @Temperature 23.0 °C |
2100 - 2500 cP @Temperature 73.4 °F |
|
Master Bond EP27 Low Temperature Curing Two Component Epoxy Master Bond Polymer System EP27 is a unique two component
epoxy formulation offers relatively fast cures at temperatures as low as 40°F and below, with curing times much shorter than currently exis.. |
|||
Viscosity | 2100 cP @Temperature 25.0 °C |
2100 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond F175 One-Part UV Curing Adhesive TRA-BOND F175 is a clear, one part UV curing adhesive designed for bonding metals, ceramics and most rigid polymers. It is an excellent adhesive for fiber optic terminations where fast cure with ult.. |
|||
Viscosity | 2100 cP @Temperature -20.0 °C |
2100 cP @Temperature -4.00 °F |
Cold Crank |
ChevronTexaco Supreme SAE 10W-30 Synthetic Motor Oil FeaturesChevron Supreme 100% Synthetic Motor Oils are designed for those drivers who demand the ultimate in engine protection. They provide an extra measure of protection for the investment in a spo.. |