Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20000 cP | 20000 cP | catalyzed with Stretch Effect B |
ACC Stretch Effect QSI Quantum Silicones Stretch Effect 22 Durometer Addition Cure Translucent Moldmaking Material
& Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, fast demold time, high elongation, excellent flexibility. Applications: special effects, skin replicat.. |
|||
Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | |
Huntsman Araldite EPN 1138 Epoxy Phenol Novolac Weight per Epoxide (EEW, g/eq) 176 to 181. Max color is 2.Comments/Applications: Epoxy phenol novolac for higher heat and chemical resistance than PY 307-1 and EPN 1139 or EPN 1179. Used in coatin.. |
|||
Viscosity | 20000 cP | 20000 cP | |
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Viscosity | 20000 cP | 20000 cP | |
Momentive Performance Materials RTV118 One Component Acetoxy Adhesive Sealant, Translucent RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Viscosity | 20000 - 25000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
20000 - 25000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2020409D8 Dielectric for Stainless Steel Dielectric is suitable for use as an insulation layer when printed and fired on to stainless steel. The thermal coefficient of expansion of this product has been matched to that of stainless steel. .. |
|||
Viscosity | 20000 - 30000 cP | 20000 - 30000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Viscosity | 20000 - 30000 cP | 20000 - 30000 cP | 30% solid in Anone/MEK |
Taiwan Sheen Soon Sheenthane® A9513H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Viscosity | 20000 cP | 20000 cP | Before Curing |
Silikony Polskie Gumosil B Silicone Rubber Flexible with low hardness |
|||
Viscosity | 20000 cP @Temperature 25.0 °C |
20000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 286-5 Latex Emulsion TRA-BOND 286-5 latex emulsion is designed for temporary sealing of molds to prevent leaking during cure. This compound will thicken gradually due to water evaporation. Store containers with caps sec.. |
|||
Viscosity | 20000 cP | 20000 cP | Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop.. |
|||
Viscosity | 20000 cP | 20000 cP | |
Dow Corning BY 11-030 Silicone Surfactant A clear dispersion of a high molecular weight silicone surfactant in cyclopentasiloxane for use in skincare, suncare, shower gel, and color cosmetic applications. INCI Name: Cyclopentasiloxane (and).. |
|||
Viscosity | 20000 cP | 20000 cP | dynamic |
Dow Corning HS II BASE & 10:1 CLEAR CATALYST High strength silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items. HS II Base with HS II 10:1 Clear Catalyst is recommended for use with polyes.. |
|||
Viscosity | 20000 cP | 20000 cP | dynamic, part A |
Dow Corning HV 1540/20P BASE AND CLEAR CURING AGENT 32 Shore, very low viscosity, castable hydrophobic silicone rubber with high tear strength and low temperature cure.Information provided by Dow Corning |
|||
Viscosity | 20000 - 80000 cP | 20000 - 80000 cP | dynamic |
Dow Corning Q2-7406 ADHESIVE Dow Corning® Q2-7406 Adhesive is a polydimethylsiloxane gum and resin dispersion; provides excellent high temperature properties with adhesion to 288C (550F).Information provided by Dow Corning |
|||
Viscosity | 20000 cP | 20000 cP | |
Armstrong A-702 Epoxy Adhesive Information provided by Ellsworth Adhesives. |
|||
Viscosity | 20000 cP | 20000 cP | |
ACC MM282 Specialist Molding 2-Part Condensation Cure Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Viscosity | 20000 cP | 20000 cP | |
ACC MM709 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Viscosity | 20000 cP | 20000 cP | |
ACC MM911 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Viscosity | 20000 cP | 20000 cP | Part B |
3M Scotchkote™ 323 Purple Patch Compound 3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple.. |
|||
Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Viscosity | 20000 - 40000 cP | 20000 - 40000 cP | |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 20000 cP @Temperature 105 °C |
20000 cP @Temperature 221 °F |
spindle #27, 18.7 grams, 5 rpm |
3M Dyneon™ FC 2210 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomers FC 2210 can be incorporated into other fluoroelastomers using standard water cooled internal mixers or two-roll mills
with standard fillers and ingredients utilized .. |
|||
Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
3M Scotch-Weld™ DP420 NS Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Viscosity | 20000 cP | 20000 cP | |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
3M Scotch-Weld™ DP405 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Viscosity | 20000 cP | 20000 cP | |
Loctite® 571 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Viscosity | 20000 cP | 20000 cP | Part B, RVT, #7, 20 rpm; TM R050-12 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |