Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 19600 cP @Shear Rate 11200 1/s, Temperature 200 °C |
19600 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |