Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 158000 cP @Temperature 25.0 °C |
158000 cP @Temperature 77.0 °F |
Mixed (sp #rv7, 20 rpm) |
Tra-Con Tra-Bond 216D01 Dam/Fill Applications Adhesive TRA-BOND 216D01 is for dam and fill applications. TRA-BOND 216D01 bonds exceptionally well to ceramic, glass, metal and plastic. Fully cured TRA-BOND 216D01 is an electrical insulator with superior .. |