Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1500 cP | 1500 cP | |
Ritelok EC1500 Gap Filling CA Adhesive Cyanoacrylate. General purpose, high viscosity adhesive. Ideal for gap filling of porous surfaces. High bond strength, High viscosity, Excellent for gap filling |
|||
Viscosity | 1500 cP | 1500 cP | |
Ritelok PR1500 Plastic & Rubber Adhesive Cyanoacrylate. Multi-purpose plastic & rubber adhesive. High strength bond & impact resistance. High bond strength, High viscosity, Excellent for gap filling |
|||
Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | |
ND Industries 542 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, fans, cams, collars, flywheels, rotors to shaftMeets military spec Mil-R-46082B Type III |
|||
Viscosity | 1500 cP @Temperature 82.2 °C |
1500 cP @Temperature 180 °F |
|
Northstar Polymers MSA-063 Polyester Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 1500 cP | 1500 cP | |
Reltek BONDiT™ B-45 Adhesive, Sealant & Coating System Key Properties: Excellent adhesive for low surface energy plastics without primer.Used in potting, painting and protective coating applications.Excellent thermal and mechanical shock resistance.Ease.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Reltek BONDiT™ B-52 Adhesive, Sealant & Potting System Key Properties: Outstanding for bonding dissimilar materials with high thermal expansion differential applications.Fast thermal cure, long pot life.Ease of use.Applications: Excellent for fast assem.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Viscosity | 1500 cP | 1500 cP | |
Resinlab® CYNERGY CA6206 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Resinlab® CYNERGY CA6306 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Viscosity | 1500 cP | 1500 cP | "B" component |
ACC QLE 1030 QSI Quantum Silicones 27 Durometer Addition Cure Elastomer for Coating
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: long pot life, excellent adhesion, 100%solid, fast cure.Applications: fabric or cloth coating. Part of the Amber Chem.. |
|||
Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV12 Clear General Purpose Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Viscosity | 1500 - 3000 cP | 1500 - 3000 cP | Part B |
Master Bond EP33CLV Epoxy Resists Chemicals and High Temperatures Description: Master Bond EP33CLV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and excel.. |
|||
Viscosity | 1500 - 1800 cP @Temperature 23.0 °C |
1500 - 1800 cP @Temperature 73.4 °F |
|
Master Bond EP37-3FLF Low Exotherm Highly Flexible Two Component Epoxy Master Bond Polymer System EP37-3FLF is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. The .. |
|||
Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond FDA8 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-8 EPOXY ADHESIVE is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food an.. |
|||
Viscosity | 1500 - 2500 cP @Temperature 23.0 °C |
1500 - 2500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7DC One Component, Dual Cure UV System Master Bond UV15-7DC is a one component, dual cure UV system for high performance bonding, sealing, coating and encapsulation applications. This system features a primary cure utilizing UV light and.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Elmer's Products Aron Alpha® 203 Cyanoacrylate Adhesive (Industrial Krazy Glue™) General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair o.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Elmer's Products Aron Alpha® 403X Cyanoacrylate Adhesive (Industrial Krazy Glue™) Engineered for high temperature and high impact resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. V.. |
|||
Viscosity | 1500 cP @Temperature 25.0 °C |
1500 cP @Temperature 77.0 °F |
|
Cytec (Conap) RN-1200 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 1500 cP | 1500 cP | |
Dow ISONATE™ 240 MDI Prepolymer ISONATE™ 240 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with a high molecular weight polyester polyol, resulting in a material with good.. |
|||
Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | MA143LFE |
C.O.I.M. FILCO® 309 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Viscosity | 1500 - 2500 cP @Temperature 35.0 °C |
1500 - 2500 cP @Temperature 95.0 °F |
|
C.O.I.M. UREXTER® T 404 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Viscosity | 1500 cP | 1500 cP | After mixing, uncured |
Atom Adhesives AA-BOND FDA8 Epoxy Adhesive AA-BOND FDA8 EPOXY ADHESIVE is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and .. |
|||
Viscosity | 1500 cP | 1500 cP | |
Abatron AboCast 8504-5 One-Component Epoxy AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera.. |
|||
Viscosity | 1500 cP | 1500 cP | dynamic |
Dow Corning DSP ANTIFOAM EMULSION 10 percent active silicone emulsion that exhibits outstanding dilution stability as well as excellent foam control persistance over a wide pH and temperature range.Information provided by Dow Cornin.. |
|||
Viscosity | 1500 cP | 1500 cP | Mixed |
Resinlab® UR3001 Clear Two Part Urethane Encapsulant Resinlab™ UR 3001 is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR 3001 provides excellent environmental p.. |
|||
Viscosity | 1500 cP | 1500 cP | Part B, RVT, #2, 20 rpm; TM R050-12 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |
|||
Viscosity | 1500 - 3000 cP | 1500 - 3000 cP | Part B |
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |
|||
Viscosity | 1500 - 3000 cP @Temperature 35.0 - 35.0 °C |
1500 - 3000 cP @Temperature 95.0 - 95.0 °F |
Average value: 2380 cP Grade Count:5 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |