Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 14300 cP @Shear Rate 10994 1/s, Temperature 210 °C |
14300 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-80-1000 TPE Product Description: StarXTRUDE XTR-80-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |
|||
Viscosity | 14300 cP @Shear Rate 10994 1/s, Temperature 210 °C |
14300 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-90-1000 TPE Product Description: StarXTRUDE XTR-90-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |