Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1200 cP | 1200 cP | Part A |
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Viscosity | 1200 cP | 1200 cP | Mixed; TM R050-12 |
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11.. |
|||
Viscosity | 1200 - 5000 cP | 1200 - 5000 cP | |
Ritelok TL22 Screwlock Anaerobic. Low strength threadlocker for fasteners less than 1/4". Prevent corrosion, Vibration resistant, Dismantle using normal tools |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
|
Northstar Polymers MSA-018 Isocyanate Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 1200 - 1800 cP @Temperature 25.0 °C |
1200 - 1800 cP @Temperature 77.0 °F |
Uncured |
Permabond 2050 Cyanoacrylate, flexible PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding.. |
|||
Viscosity | 1200 - 2400 cP @Temperature 25.0 °C |
1200 - 2400 cP @Temperature 77.0 °F |
Uncured |
Permabond 268 Cyanoacrylate, General purpose PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano.. |
|||
Viscosity | 1200 cP | 1200 cP | |
Resinlab® TL5022 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Viscosity | 1200 - 2500 cP @Temperature 25.0 °C |
1200 - 2500 cP @Temperature 77.0 °F |
Uncured |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Viscosity | 1200 - 2000 cP | 1200 - 2000 cP | |
Huntsman Araldite XB 4383-1 Brominated Resin Weight per Epoxide (EEW, g/eq) 317 to 345. Max color is 6.Comments/Applications: For use in the manufacturing of thin laminates, prepregs and rigid laminates for printed wiring boards requiring fla.. |
|||
Viscosity | 1200 cP | 1200 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1173 B (SIBS) Linear Triblock Copolymer Description: Kraton D1173 B is a clear, linear triblock copolymer based on styrene, butadiene and isoprene with a polystyrene content of 18%. It is supplied from Brazil in the form: Kraton D1173 BT .. |
|||
Viscosity | 1200 cP @Shear Rate 100 1/s, Temperature 180 °C |
1200 cP @Shear Rate 100 1/s, Temperature 356 °F |
Melt |
Metabolix Mirelâ„¢ P4001 Sheet Extrusion Grade Bioplastic Mirelâ„¢ P4001 is a general purpose, high melt strength material suitable for cast sheet extrusion. Mirelâ„¢ P4001 is designed for a wide range of sheet applications including gift cards, prom.. |
|||
Viscosity | 1200 - 1800 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200 - 1800 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2000511D1 Platinized Carbon Ink Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working e.. |
|||
Viscosity | 1200 cP @Temperature 40.0 °C |
1200 cP @Temperature 104 °F |
|
Solvay DURAPHOS® 178 Surfactant Identification: ALKYL AMINE NEUTRALIZED ORGANIC PHOSPHATECAS: 68187-67-7Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: DURAPHOS© 178 is a concentrated amine neut.. |
|||
Viscosity | 1200 cP | 1200 cP | 1.3% NaCl added |
Solvay MACKADET® CA-ND Surfactant Product description: Mackadet CA-ND is a concentrated blend of mild surfactants for use as a base for high foaming surfactant systems. Mackadet CA-ND responds rapidly to viscosity building with the .. |
|||
Viscosity | 1200 - 1500 cP | 1200 - 1500 cP | |
Master Bond Mastersil 151 Two Component Low Viscosity Silicone Compound Master Bond MasterSil 151 is a two component, low viscosity
silicone compound for high performance potting and
encapsulation. MasterSil 151 is an addition cured system and does not require exposure.. |
|||
Viscosity | 1200 - 1850 cP @Temperature 125 °C |
1200 - 1850 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® N-10 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-10 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre.. |
|||
Viscosity | 1200 - 1500 cP @Temperature 23.9 °C |
1200 - 1500 cP @Temperature 75.0 °F |
|
TSE Industries EzNATE® 200 Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Viscosity | 1200 - 6000 cP | 1200 - 6000 cP | Thixotropic |
Loctite® 242 Medium Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
|
Cytec Conathane® CE-1175 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Viscosity | 1200 - 1700 cP @Temperature 23.0 °C |
1200 - 1700 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OG142-112 UV Cure Optical Epoxy Material Description: Single component, medium viscosity, UV curable epoxy for adhesive sealing and encapsulating fiber optic and optoelectronic packaging application. Replacement version of EPO-TE.. |
|||
Viscosity | 1200 cP | 1200 cP | |
Dymax 3089 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | <= 1200 cP | <= 1200 cP | |
Abatron AboTar 8101-8 Solventless Tar-Epoxy Compound AboTar 8101-8 is a 2-part tar-epoxy variable-ratio system. It is weather- and water-proof, flexible, and acid, alkali, and fuel resistant. It can be used neat or with sand or aggregates. Uses: Resu.. |
|||
Viscosity | 1200 cP | 1200 cP | "B" component |
ACC QLE 1031 QSI Quantum Silicones 25 Durometer Addition Cure Elastomer for Coating QLE 1031 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Viscosity | 1200 cP | 1200 cP | Part A |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Viscosity | 1200 cP | 1200 cP | Part B |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Viscosity | 1200 cP | 1200 cP | |
Resinlab® TL5042 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Viscosity | 1200 - 2200 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200 - 2200 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2090130P5 Pink Dielectric Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |