Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 11500 cP @Shear Rate 10994 1/s, Temperature 210 °C |
11500 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7195-1000 TPE Product Description: StarFlex P 7195-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Viscosity | 11500 cP @Shear Rate 10994 1/s, Temperature 210 °C |
11500 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7050-1000 TPE Product Description: StarMediflex P 7050-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Viscosity | 11500 - 15000 cP | 11500 - 15000 cP | |
Beijing Ranger Chem SM-828 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 11500 - 15000 cP | 11500 - 15000 cP | |
Beijing Ranger Chem SM-828H Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 11500 cP @Temperature 177 °C |
11500 cP @Temperature 350 °F |
Typical |
Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue StickMedium performance. Oil resistance for wood, fabric and other porous substrates primarily in woodworking assembly operation. |