Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 100000 - 200000 cP | 100000 - 200000 cP | |
Palm Labs Adhesives Turbo Anti-Seize Copper Paste TURBO ANTI-SEIZE – COPPER is a copper, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where prot.. |
|||
Viscosity | 100000 cP @Temperature 260 °C |
100000 cP @Temperature 500 °F |
melt; 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Viscosity | 100000 - 300000 cP @Temperature 25.0 °C |
100000 - 300000 cP @Temperature 77.0 °F |
Uncured |
Permabond ES558 Epoxy Resin PERMABOND ES558 is a single-part epoxy paste which flows like solder when heated during curing. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear strength... |
|||
Viscosity | 100000 cP | 100000 cP | RVT, #6, 2.5 rpm; TM R050-12 |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Viscosity | 100000 - 295000 cP | 100000 - 295000 cP | Average value: 233000 cP Grade Count:12 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Viscosity | 100000 - 300000 cP | 100000 - 300000 cP | |
Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Viscosity | 100000 - 300000 cP | 100000 - 300000 cP | |
Lord Adhesives 406 Flexible, High Impact and Peel Resistance, Medium Working Time Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Viscosity | 100000 - 125000 cP | 100000 - 125000 cP | A |
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Viscosity | 100000 cP | 100000 cP | Melt Viscosity; SABIC Method |
SABIC Innovative Plastics Valox® 305 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 1450-1850. |
|||
Viscosity | 100000 cP | 100000 cP | |
Shin-Etsu Silicones KE-347TUV Silicone, RTV Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 100000 cP | 100000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | |
Master Bond LED401 One Component LED Curable Adhesive System Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | |
Master Bond LED403Med USP Class VI, One Component, LED Curable System Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi.. |
|||
Viscosity | 100000 cP @Temperature 25.0 °C |
100000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2116 Low Vapor Pressure Epoxy Staking Compound TRA-BOND 2116 is a thixotropic, low vapor pressure epoxy system that passes the NASA Outgassing Specification. It is recommended for critical electronic, aerospace, and industrial applications where.. |
|||
Viscosity | >= 100000 cP | >= 100000 cP | Part B |
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F Description: Master Bond Polymer System Supreme 11HT-LO is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room .. |
|||
Viscosity | 100000 cP @Temperature 160 °C |
100000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 100000 cP | 100000 cP | |
Cotronics 454B Machinable Non-Sag Putty Adhesive |
|||
Viscosity | 100000 - 6.00e+6 cP | 100000 - 6.00e+6 cP | |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Viscosity | 100000 - 6.00e+6 cP | 100000 - 6.00e+6 cP | |
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Viscosity | 100000 cP | 100000 cP | |
3M Scotch-Weld™ DP5001 Structural Adhesive Flexible and Conveyor belt repairInformation provided by 3M |
|||
Viscosity | 100000 cP | 100000 cP | Melt |
3M Dyneon™ TF 9205 PTFE 3M™ Dyneon™ PTFE TF micropowders can be used as additives in many different applications and at concentrations typically from 5 to 20%. Homogeneous incorporation helps ensure optimum performance. .. |
|||
Viscosity | 100000 - 120000 cP @Temperature 23.0 °C |
100000 - 120000 cP @Temperature 73.4 °F |
|
Master Bond Supreme 45HTQ Quartz Filled, Heat Resistant Epoxy Compound Master Bond Polymer Adhesive Supreme 45HTQ is a two component, toughened, quartz filled epoxy compound for high performance structural bonding and casting. It is suitable for applications where long.. |
|||
Viscosity | 100000 - 125000 cP | 100000 - 125000 cP | A |
ITW Plexus Plexus™ MA922 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works. |
|||
Viscosity | 100000 - 125000 cP | 100000 - 125000 cP | A |
ITW Plexus Plexus™ MA925 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works. |
|||
Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | Part A |
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |