Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 10.5 - 18 cP | 10.5 - 18 cP | |
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete Primkote G is a waterborne epoxy system for priming and sealing floors. It contains a gray resin compound (Part A) and a clear hardener (Part B). It conditions concrete and other substrates for epox.. |