Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.00e+6 cP @Shear Rate 270 1/s, Temperature 230 °C |
1.00e+6 cP @Shear Rate 270 1/s, Temperature 446 °F |
|
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows .. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 190 1/s, Temperature 230 °C |
1.00e+6 cP @Shear Rate 190 1/s, Temperature 446 °F |
|
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%... |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 11E573 Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 - 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 - 716 °F |
Average value: 5.50e+6 cP Grade Count:5 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Average value: 5.50e+6 cP Grade Count:10 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | Melt |
3M Dyneon™ TF 9207 PTFE
(discontinued **) Low molecular weight virgin PTFEAgglomerate particlesEasily deagglomeratedInformation provided by Dyneon, A 3M Company |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | Gum Viscosity |
Shin-Etsu Silicones KF-9004 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2001-50A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Elvax® 3190 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F132 PA6 Film Extrusion, High Viscosity |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-230ASL PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc... |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
1.00e+6 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® XP32-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 cP | 1.00e+6 cP | Melt Velocity |
Asahi Glass Fluon® ETFE A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
DuPont Bynel® 3933 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Viscosity | 1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
1.00e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Elvax® 3173SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
(discontinued **)< 18 wt% Vinyl Acetate.Elvax® 3173SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |