Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20 - 80 cP | 20 - 80 cP | |
Huntsman Kerimid 701-1 B US Resin Comments/Applications: Used with Kerimid 701 A US for high Tg laminate systems. Suggested ratio 3 parts A to 1 part B.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acq.. |
|||
Viscosity | 70 - 80 cP @Temperature 20.0 °C |
70 - 80 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-75 Polyvinyl Alcohol Fully Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |
|||
Viscosity | 30 - 80 cP | 30 - 80 cP | |
Beijing Ranger Chem 6690-3 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 40 - 80 cP | 40 - 80 cP | |
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C) |
|||
Viscosity | 40 - 80 cP | 40 - 80 cP | |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |