Polymer Property : Viscosity = 650000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 650000 - 650000 cP

@Temperature 420 - 420 °C
650000 - 650000 cP

@Temperature 788 - 788 °F
Average value: 650000 cP Grade Count:1
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
Viscosity 510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-810 Polyetheretherketone (PEEK)
KetaSpire® KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades ..
Viscosity 510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-810FP Polyetheretherketone (PEEK)
KetaSpire® KT-810FP is the fine powder form of KT-810 resin. KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0..