Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 640000 - 640000 cP @Temperature 117 - 117 °C |
640000 - 640000 cP @Temperature 243 - 243 °F |
Average value: 640000 cP Grade Count:1 |
Overview of materials for Polybutene This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |