Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 300 - 500 cP | 300 - 500 cP | |
ND Industries 444 High pressure Sealant Very high strength hydraulic sealant. Non-shrink, high vibration and shock resistance |
|||
Viscosity | 100 - 500 cP | 100 - 500 cP | |
ND Industries 530 Shaft & Bearing Retainer Retaining Compound General DescriptionA high strength adhesive for retention of cylindrical components, where disassembly is not required.Typical Usesrotors, shafts, bushings, bearings, and pulleysMeets military spec .. |
|||
Viscosity | 90 - 500 cP @Temperature 25.0 °C |
90 - 500 cP @Temperature 77.0 °F |
|
Northstar Polymers MNB-013 Isocyanate Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Huntsman AroCy XU 379 Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman. |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Huntsman HY 360 Polyamide Approx. H+ equivalent weight 134. Mix Ratio with GY 6010 is 60.Comments/Applications: Very low viscosity, modified polyamidoamine; compatible with bis F resins. Superior chemical resistance. Ult.. |
|||
Viscosity | 290 - 500 cP | 290 - 500 cP | |
Huntsman HY 956 Aliphatic Amine Approx. H+ equivalent weight 47. Mix Ratio with GY 6010 is 25.Comments/Applications: Low viscosity liquid amine with low shrinkage, excellent dimensional stability, good electricals. Adhesives, c.. |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | As Supplied |
Heraeus Cleviosâ„¢ S HT Antistatic/Conductive Polymer Coating for Screen Printing Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as a paste designed for application by silk screen printing to be used for transparent conductive devices. Cleviosâ„¢ S HT grade .. |
|||
Viscosity | 400 - 500 cP @Temperature 23.0 °C |
400 - 500 cP @Temperature 73.4 °F |
|
Master Bond EP30 Optically Clear, Low Viscosity Two Component Epoxy Master Bond Polymer System EP30 is a low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at room temperature or more.. |
|||
Viscosity | 280 - 500 cP | 280 - 500 cP | Part B |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | Part B |
Master Bond EP30HV Optically Clear, High Strength Two Part Epoxy Description: Master Bond EP30HV is a lower viscosity, two component epoxy system for high performance bonding, sealing, coating and potting. It is formulated to cure at room temperature or more rapi.. |
|||
Viscosity | 200 - 500 cP | 200 - 500 cP | NOV QC 020 |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 300 - 500 cP @Temperature 23.0 °C |
300 - 500 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. .. |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
C.O.I.M. FILCO® 300 Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber Sizing Description: Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in.. |
|||
Viscosity | 200 - 500 cP | 200 - 500 cP | |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
Viscosity | 350 - 500 cP | 350 - 500 cP | |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Viscosity | 350 - 500 cP | 350 - 500 cP | blended |
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Viscosity | 200 - 500 cP | 200 - 500 cP | Mixed Viscosity |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | blended |
Abatron AboCast 7802-1/AboCure 50-12 Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-12 is a clear converter for high rigidity, chemical, and temperature resistance (HDT: 101.. |
|||
Viscosity | 30.0 - 500 cP @Temperature 230 - 270 °C |
30.0 - 500 cP @Temperature 446 - 518 °F |
Average value: 188 cP Grade Count:2 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Viscosity | 200 - 500 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
200 - 500 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080529D7 Carbon Flexographic Ink Carbon conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and go.. |