Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 360000 - 360000 cP @Temperature 250 - 250 °C |
360000 - 360000 cP @Temperature 482 - 482 °F |
Average value: 221000 cP Grade Count:1 |