Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 250000 - 350000 cP @Temperature 400 - 400 °C |
250000 - 350000 cP @Temperature 752 - 752 °F |
Average value: 300000 cP Grade Count:2 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Viscosity | 550 - 350000 cP | 550 - 350000 cP | Average value: 27500 cP Grade Count:27 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |
|||
Viscosity | 350000 - 350000 cP @Temperature 200 - 200 °C |
350000 - 350000 cP @Temperature 392 - 392 °F |
Average value: 223000 cP Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Viscosity | 100000 - 350000 cP | 100000 - 350000 cP | |
Lord Adhesives 403 Flexible, High Impact and Peel Resistance, Fast Cure Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Viscosity | 100000 - 350000 cP | 100000 - 350000 cP | |
Lord Adhesives 410 Flexible, High Impact and Peel Resistance, Long Working Time Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Viscosity | 225000 - 350000 cP | 225000 - 350000 cP | Part B |
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick.. |
|||
Viscosity | 150000 - 350000 cP @Temperature 230 - 290 °C |
150000 - 350000 cP @Temperature 446 - 554 °F |
Average value: 213000 cP Grade Count:1 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Viscosity | 150000 - 350000 cP @Shear Rate 0.100 - 1000 1/s |
150000 - 350000 cP @Shear Rate 0.100 - 1000 1/s |
Average value: 213000 cP Grade Count:1 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |