Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 170 - 210 cP @Temperature 60.0 °C |
170 - 210 cP @Temperature 140 °F |
|
C.O.I.M. DIEXTER® G680 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 130 - 210 cP @Temperature 25.0 °C |
130 - 210 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PA-26 MDI Isocyanate Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyether-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for .. |
|||
Viscosity | 150 - 210 cP @Temperature 25.0 °C |
150 - 210 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PA-28 MDI Isocyanate Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyether-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for p.. |