Polymer Property : Viscosity = 2.70e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2.20e+6 - 2.70e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.20e+6 - 2.70e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Viscosity 2.20e+6 - 2.70e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.20e+6 - 2.70e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Viscosity 2.30e+6 - 2.70e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.30e+6 - 2.70e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Viscosity 2.30e+6 - 2.70e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
2.30e+6 - 2.70e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 2801-00 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi..