Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 7000 - 19000 cP | 7000 - 19000 cP | |
Huntsman MY 720 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: Tetra-functional liquid epoxy based on methylene dianiline. Excellent high temperature, chemical and radiation resista.. |
|||
Viscosity | 11000 - 19000 cP @Shear Rate 100 1/s, Temperature 25.0 °C |
11000 - 19000 cP @Shear Rate 100 1/s, Temperature 77.0 °F |
Haake VT550 cone and plate viscometer (PK1.1°) |
Gwent Electronic Materials C2000107P3 Silver Ink Silver Ink C2000107P3 is designed as a termination for single layer PZT ceramics. After firing the film has good adhesion and solderability.The ink is in a ready to use form at a viscosity suitable.. |
|||
Viscosity | 17000 - 19000 cP | 17000 - 19000 cP | |
Huntsman MY 9663 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 115 to 135. Color: BrownComments/Applications: Narrow viscosity MY 720. Used for high performance composites, adhesives, laminates and high energy radiation resistant.. |