Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 80 - 105 cP @Temperature 25.0 °C |
80 - 105 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® 9 General Purpose Catalyst Emerson & Cuming 9 Eccobond® General Purpose CatalystGeneral purpose, low viscosity. Imparts good physical strength and chemical resistance to cured castings. Recommended for most general purpose a.. |
|||
Viscosity | 85 - 105 cP | 85 - 105 cP | ASTM D445 |
ExxonMobil Jayflex™ DINP Plasticizer (European Grade) Availability: Europe, Middle East & AfricaCAS Number: 68515-48-0EC Number: 271-090-9Information provided by ExxonMobil |