Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 - 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 - 716 °F |
Average value: 5.50e+6 cP Grade Count:5 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Average value: 5.50e+6 cP Grade Count:10 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-230ASL PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc... |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EA-LR43 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-610 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-610AS ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-210 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided .. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 380 °C |
1.00e+6 - 1.00e+7 cP @Temperature 716 °F |
Melt viscosity |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Viscosity | 1.00e+6 - 1.00e+7 cP @Temperature 300 - 330 °C |
1.00e+6 - 1.00e+7 cP @Temperature 572 - 626 °F |
Melt viscosity |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |