Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 9200 - 9800 cP | 9200 - 9800 cP | |
Huntsman Tactix 138 Epoxy Weight per Epoxide (EEW, g/eq) 178 to 182.Comments/Applications: Low viscosity epoxy resin for applications such as filament winding.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemical.. |
|||
Viscosity | 9200 cP @Shear Rate 10994 1/s, Temperature 210 °C |
9200 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |