Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 900000 - 3.00e+6 cP @Temperature 190 - 190 °C |
900000 - 3.00e+6 cP @Temperature 374 - 374 °F |
Average value: 1.60e+6 cP Grade Count:15 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Viscosity | 900000 - 3.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
900000 - 3.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 1.60e+6 cP Grade Count:15 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Viscosity | >= 900000 cP | >= 900000 cP | Part B, thixotropic |
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or .. |
|||
Viscosity | 900000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
900000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Viscosity | 900000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
900000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 1123 Modified EVA Adhesive Resin Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Viscosity | 900000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
900000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 3810 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Viscosity | 900000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
900000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |