Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 850000 cP | 850000 cP | Mixed; TM R050-12 |
Resinlab® EP1121-4 Adhesive / Casting Resin Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives .. |
|||
Viscosity | 850000 cP @Shear Rate 190 1/s, Temperature 230 °C |
850000 cP @Shear Rate 190 1/s, Temperature 446 °F |
|
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo.. |
|||
Viscosity | 850000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
850000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Viscosity | 850000 cP @Temperature 400 °C |
850000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Viscosity | 850000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
850000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Viscosity | 850000 cP | 850000 cP | Mixed |
Armstrong A-4/A Epoxy Adhesive Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe.. |