Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 8000 cP @Temperature 190 °C |
8000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 3180 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Propylene homopolymer and FDA compliantFeatures: Temperature resistance, high melt viscosity, and increased hardnessApplications: Component of modified bi.. |
|||
Viscosity | 8000 - 800000 cP @Temperature 230 - 270 °C |
8000 - 800000 cP @Temperature 446 - 518 °F |
Average value: 187000 cP Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Viscosity | 8000 cP @Temperature 190 °C |
8000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 2180 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point, short open time, good cohesive strength, and high viscosityApplications: Component of h.. |
|||
Viscosity | 8000 - 11000 cP | 8000 - 11000 cP | |
Huntsman XU MY 722 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 117 to 134. Color: BrownComments/Applications: New chemistry; lowest viscosity tetra-functional epoxy resin overall. Room temperature stable. Used for composites, a.. |
|||
Viscosity | 8000 cP | 8000 cP | Mixed Viscosity |
ITW Devcon 2 Ton® Epoxy Clear Epoxy, Clear, White Information provided by ITW Devcon |
|||
Viscosity | 8000 - 10000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
8000 - 10000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2070920D1 Depolymerisable Carbon Ink This product is designed as a screen printable ink. This product is based on a thermoplastic resin system designed to burn out completely during firing to leave a void of specific shape and dimensi.. |
|||
Viscosity | 8000 - 15000 cP @Temperature 40.0 °C |
8000 - 15000 cP @Temperature 104 °F |
|
Taiwan PU Corporation PPG CPU-2095 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Viscosity | 8000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
8000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7350-9000 TPE Product Description: StarFlex P 7350-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Metho.. |
|||
Viscosity | 8000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
8000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7370-1000 TPE Product Description: StarFlex P 7370-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Viscosity | 8000 - 10000 cP @Temperature 23.0 °C |
8000 - 10000 cP @Temperature 73.4 °F |
|
Master Bond EP62-1 High Glass Transition Temperature Epoxy System Master Bond EP62-1 is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. The cured epoxy resin ex.. |
|||
Viscosity | 8000 cP @Temperature 23.0 °C |
8000 cP @Temperature 73.4 °F |
|
Master Bond UV14-3 Flexible, UV Curable Adhesive System Master Bond UV14-3 is a one component, flexible, UV curable polymer system for bonding, sealing and coating with the convenient feature of being readily removable by most conventional solvents. It i.. |
|||
Viscosity | 8000 cP @Temperature 25.0 °C |
8000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® 2072 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Viscosity | 8000 - 10000 cP @Temperature 23.0 °C |
8000 - 10000 cP @Temperature 73.4 °F |
|
Master Bond UV15TK High Temperature Resistant One Component UV Curable System Master Bond UV15TK is a moderate viscosity, epoxy based UV curable system for bonding, sealing and coating. It is 100% reactive and does not contain any solvents or other volatiles. It is also compl.. |
|||
Viscosity | 8000 - 12000 cP @Temperature 23.0 °C |
8000 - 12000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide Product Description: EPO-TEK® P-1011 is a single component, modified polyimide, silver-filled adhesive designed for chip bonding in microelectronic and optoelectronic applications.Advantages & Appl.. |
|||
Viscosity | 8000 cP | 8000 cP | dynamic |
Dow Corning 1430 ANTIFOAM Stable at high and low pH. Dow Corning® Antifoam 1430 is a water-dilutable, 30 percent active silicone emulsion that is designed to control foam in aqueous systems.Information provided by Dow Corni.. |
|||
Viscosity | 8000 cP | 8000 cP | dynamic |
Dow Corning 3629 Two Part LSR SystemInformation provided by Dow Corning |
|||
Viscosity | 8000 cP @Temperature 25.0 °C |
8000 cP @Temperature 77.0 °F |
|
Abatron AboCast/AboCure 50-24/8501-4 High Temperature Resistant Epoxy Clear amber, low viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to.. |
|||
Viscosity | <= 8000 cP | <= 8000 cP | |
Abatron AboTar 8607-1 Solventless Tar-Epoxy Compound AboTar 8607-1 is a 2-part tar-epoxy lower cost system for filling and leveling pot holes and grossly uneven flooring. It can be used neat or with sand or aggregates. Uses: Resurfacing concrete and .. |
|||
Viscosity | 8000 - 14000 cP | 8000 - 14000 cP | Accelerator |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Viscosity | 8000 - 12000 cP | 8000 - 12000 cP | |
Beijing Ranger Chem SM-827H Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 8000 - 15000 cP | 8000 - 15000 cP | |
Beijing Ranger Chem SM-601RX75 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 8000 cP | 8000 cP | Part A, RVT, #5, 20 rpm; TM R050-12 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Viscosity | 8000 cP | 8000 cP | Mixed; TM R050-12 |
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Viscosity | 8000 cP | 8000 cP | Severs, 100 psig aged 2 hrs, See note 1; SPI-VD-T2 |
Formosa Plastics Formolon® NVA PVC PVC Homopolymer Dispersion Resin F-NVA is a high molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Plastisols containing F-NVA exhibit low paste viscosities and.. |
|||
Viscosity | 8000 - 11000 cP | 8000 - 11000 cP | |
Beijing Ranger Chem HY-127 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | <= 8000 cP | <= 8000 cP | #3 SP @ 12 rpm; RP-0596 |
Solvay RHODAPEX® EA-2 Surfactant Description: Primary surfactant used in shampoos, bubble baths, shin cleansers and related cosmetic products. For use in both hard and soft water.Chemical Name: AMMONIUM LAURETH SULFATECAS: 67762-19.. |
|||
Viscosity | 8000 cP @Temperature -15.0 °C |
8000 cP @Temperature 5.00 °F |
Cold Crank |
ChevronTexaco Havoline® SAE 20W-50 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |