Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 54000 cP @Temperature 25.0 °C |
54000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a.. |
|||
Viscosity | 54000 cP | 54000 cP | uncured |
Atom Adhesives AA-BOND F162 Epoxy Adhesive AA-BOND F162 is a thixotropic electrical insulating epoxy adhesive system with low vapor pressure and outgassing characteristics. AA-BOND F162 was specifically developed for fiber optic, laser, phot.. |