Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5000 cP @Pressure 0.621 MPa |
5000 cP @Pressure 90.0 psi |
Servers; ASTM D-1823 |
SABIC PVC 673E Emulsion Polyvinyl Chloride Product Description: PVC 673E is a fine particle, medium-molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting high viscosi.. |
|||
Viscosity | 5000 cP | 5000 cP | |
NextGen Adhesives M907-20 Medical Grade Epoxy Adhesive Description: NGAC M907-20 is a medium viscosity adhesive system that is specifically formulated for medical device assembly applications.Advantages and Applications: Uses include laminating, bonding.. |
|||
Viscosity | 5000 cP | 5000 cP | Mixed; TM R050-12 |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Viscosity | 5000 cP @Temperature 25.0 °C |
5000 cP @Temperature 77.0 °F |
Uncured |
Permabond HH040 Anaerobic Retainer Permabond® HH040 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitiz.. |
|||
Viscosity | 5000 - 35000 cP @Temperature 60.0 - 60.0 °C |
5000 - 35000 cP @Temperature 140 - 140 °F |
Average value: 20000 cP Grade Count:3 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Viscosity | 5000 - 7000 cP | 5000 - 7000 cP | |
Huntsman Araldite GY 281 Bisphenol F Epoxy Resin Weight per Epoxide (EEW, g/eq) 159 to 172. Max color is 4.Comments/Applications: Unmodified, low viscosity bis F epoxy, good flexibility. FDA listed. Used in coatings, adhesives, tank linings, fl.. |
|||
Viscosity | 5000 - 6800 cP | 5000 - 6800 cP | |
Huntsman Araldite GY 6004 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 178 to 196. Max color is 1.Comments/Applications: Slightly modified GY 6010. Medium viscosity, general purpose, highly versatile resin for use in cold or heat-cured .. |
|||
Viscosity | <= 5000 cP | <= 5000 cP | |
Hybrid Plastics POSS® EP 1000 Epoxy Adhesive EP1000 is a POSS® based epoxy adhesive with outstanding oxidative resistance to ozone, plasma, or atomic oxygen environments. The EP1000 POSS® Epoxy is also well-suited for peroxide and steam... |
|||
Viscosity | 5000 cP | 5000 cP | BAM 922 |
Kraton® FG1901 G (SEBS) grafted with MA Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form id.. |
|||
Viscosity | 5000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
5000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-9000 TPE Product Description: StarGrip GP 25-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubber.. |
|||
Viscosity | 5000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
5000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 30-9000 TPE Product Description: StarGrip GP 30-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
Viscosity | 5000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
5000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 45-1000 TPE Product Description: StarGrip GP 45-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
Viscosity | 5000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
5000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 55-1000 TPE Product Description: StarGrip GP 55-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
Viscosity | <= 5000 cP | <= 5000 cP | #4 SP @ 20 rpm; RP-0659 |
Solvay MIRACARE® BC-20 Surfactant Description: MIRACARE BC-20 is a concentrated baby shampoo formula which yields a finished product upon dilution. MIRACARE BC-20 retains the traditional ultra-mild shampoo ingredients, while combini.. |
|||
Viscosity | <= 5000 cP | <= 5000 cP | #4 sp @ 60 rpm; RP-0596 |
Solvay RHODOLINE® OTE 500 Surfactant Description: Open time additive for zero to low VOC paints.Identification: DEFOAMER BLENDAvailable in: Asia Pacific, Europe, Latin America and North America.Applications: RHODOLINE© OTE 500 is a.. |
|||
Viscosity | 5000 cP @Temperature 25.0 °C |
5000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 342-1 Room Temperature Cure Epoxy Adhesive TRA-BOND 342-1 room temperature curing epoxy adhesive is designed for applications which require outstanding thermal shock properties. This adhesive may be used to bond semi-porous materials, such a.. |
|||
Viscosity | 5000 cP @Temperature 25.0 °C |
5000 cP @Temperature 77.0 °F |
Mixed (sp #6, 10 rpm) |
Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound TRA-CAST 3104 is a low viscosity, room temperature cure epoxy casting system developed for high performance production encapsulation and impregnating applications where filling fine intricate free s.. |
|||
Viscosity | 5000 - 6000 cP @Temperature 23.0 °C |
5000 - 6000 cP @Temperature 73.4 °F |
|
Master Bond EP34CA Low Viscosity Heat Resistant Epoxy System Master Bond EP34CA is a low viscosity, polyfunctional, heat resistant epoxy resin designed for use in high performance composite structures, potting and casting applications. EP34CA can be used up t.. |
|||
Viscosity | >= 5000 cP | >= 5000 cP | |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix HexPly® M49 is a 120°C curing toughened epoxy matrix with good impact resistance suitable for use in performance cars. The matrix is highly tolerant of a wide variety of production techniques and .. |
|||
Viscosity | 5000 cP | 5000 cP | |
Loctite® PRISM® 411 Clear Instant Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 5000 cP | 5000 cP | |
Cotronics Bond-It™ 7040 Epoxy, Room Temperature Cure Forms high strength bonds to difficult metals, plastics, glass, ceramics, composites, etc. Cures at room temperature with high temperature strength and good electrical and thermal shock resistance... |
|||
Viscosity | 5000 cP | 5000 cP | STD |
Dymax 625 Structural Adhesive Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in SecondsMulti-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products .. |
|||
Viscosity | 5000 cP | 5000 cP | |
Dymax 956 Potting and Encapsulation Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 956 Potting and Encapsulation AdhesiveHigh strength and flexible, excellent for bonding dissimilar substrates Cure T.. |
|||
Viscosity | 5000 - 15000 cP | 5000 - 15000 cP | |
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
|||
Viscosity | 5000 cP | 5000 cP | uncured |
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive AA-SUPERTHERM 195 is a two component, thermally conductive epoxy system recommended for staking transistors, diodes, resistors, integrated circuits and other heat sensitive components to printed cir.. |
|||
Viscosity | 5000 cP | 5000 cP | Part B, RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1300 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Black (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |