Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 332000 cP | 332000 cP | Mixed (rv #7, 10 rpm) |
Tra-Con Tra-Bond 216H01 Blush-Free Non-Sag Structural Epoxy Adhesive TRA-BOND 216H01 is a two-part epoxy adhesive specifically formulated to be non-sagging and have improved adhesion to smooth, non-porous substrates such as glass, ceramic, stainless steel, etc. This .. |