Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG47 ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG47F ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG47N ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 240°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® MGABS02 ABS General purpose ABS. Excellent flow/impact. |
|||
Viscosity | 225000 cP | 225000 cP | Melt Viscosity, 260°C, 1000 sec-1; ASTM D3825 |
SABIC Innovative Plastics Cycolac® X11 ABS Automotive: High heat resistance. Excellent flow/impact balance. UL94 HB rated. High gloss. |
|||
Viscosity | 225000 cP @Temperature 260 °C |
225000 cP @Temperature 500 °F |
melt; 1000 sec-1; ASTM D 3825 |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Viscosity | 225000 cP @Temperature 420 °C |
225000 cP @Temperature 788 °F |
melt; ISO 11443 |
Victrex® ST™ P45 PolyEtherKetoneEtherKetoneKetone (PEKEKK), High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, coarse powder for extrusion compounding, low flow, color natural.Information Provid.. |
|||
Viscosity | 225000 cP @Temperature 420 °C |
225000 cP @Temperature 788 °F |
melt; ISO 11443 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Viscosity | 225000 - 255000 cP @Temperature 260 - 260 °C |
225000 - 255000 cP @Temperature 500 - 500 °F |
Average value: 245000 cP Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Viscosity | 225000 - 350000 cP | 225000 - 350000 cP | Part B |
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick.. |