Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 180 - 220 cP | 180 - 220 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 140 (200 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 140 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 180 - 260 cP | 180 - 260 cP | |
LG Chemical CP-ST Advantage: Super slump retention; Low concrete viscosity; Good combination with water reducer (WRM, WB, RS)Main Uses: Super slump retentionInformation provided by LG Chemical |
|||
Viscosity | 180 cP | 180 cP | |
Solvay SIPOMER® SEM 25 Polyalkoxyl Polyarylphenol Ethylenic Methacrylate Description: Specialty monomer for Rheology modificationChemical Name: POLYALKOXYL POLYARYLPHENOL ETHYLENIC METHACRYLATECAS: 79-41-4Available in: Asia Pacific, Europe, Latin America and North Americ.. |
|||
Viscosity | 180 cP @Temperature 25.0 °C |
180 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive TRA-BOND F113 is an optically clear, low viscosity, high impact epoxy adhesive developed for bonding and small volume potting of plastic or glass optical fibers, lenses, and prisms, LED displays, an.. |
|||
Viscosity | 180 - 460 cP | 180 - 460 cP | NOV QC 020 |
Lubrizol ESTANE® 5702F3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 180 cP @Temperature 25.0 °C |
180 cP @Temperature 77.0 °F |
|
Dow SPECTRIM™ MM 310-A Isocyanate SPECTRIM™ MM 310-A specialty isocyanate is a component of SPECTRIM™ MM 310 reaction moldable polymer.Information provided by Dow |
|||
Viscosity | 180 cP @Temperature 30.0 °C |
180 cP @Temperature 86.0 °F |
|
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor.. |
|||
Viscosity | 180 cP | 180 cP | ASTM-D562 |
Abatron Epotron 5 Clear Liquid Epoxy Adhesive for Structural Bonding Epotron 5 is a clear liquid epoxy adhesive for structural bonding. It is recommended for high-strength, permanent bonding of metal, ceramic, glass, laminates, and most rigid materials. Features: Hi.. |