Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 175000 - 850000 cP @Temperature 400 - 420 °C |
175000 - 850000 cP @Temperature 752 - 788 °F |
Average value: 513000 cP Grade Count:11 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Viscosity | 175000 cP @Temperature 400 °C |
175000 cP @Temperature 752 °F |
Melt; ISO 11443 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Viscosity | 175000 - 220000 cP | 175000 - 220000 cP | A |
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois .. |
|||
Viscosity | 175000 - 220000 cP | 175000 - 220000 cP | B |
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois .. |
|||
Viscosity | 175000 cP | 175000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Viscosity | >= 175000 cP @Temperature 23.0 °C |
>= 175000 cP @Temperature 73.4 °F |
|
Master Bond EP21BAS Radiopaque Two Component Epoxy Master Bond Polymer System EP21BAS is a radiopaque epoxy compound which offers outstanding performance and superior processability. Radiopaque epoxy polymer compounds are employed for medical diagno.. |
|||
Viscosity | 175000 cP @Temperature 250 °C |
175000 cP @Temperature 482 °F |
@ 1000 sec-1; ISO 11443 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Viscosity | 175000 cP @Temperature 250 °C |
175000 cP @Temperature 482 °F |
@ 1000 sec-1; ISO 11443 |
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Viscosity | 175000 - 275000 cP @Temperature 23.0 °C |
175000 - 275000 cP @Temperature 73.4 °F |
1 rpm |
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p.. |
|||
Viscosity | 175000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
175000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 175000 cP | 175000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East) VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |