Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1200 cP | 1200 cP | Part B, RVT, #2, 20 rpm; TM R050-12 |
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11.. |
|||
Viscosity | 1200 - 1500 cP | 1200 - 1500 cP | Thixotropic |
ND Industries ScrewGrade® 111 Removable Threadlocker A low strength threadlocker which eliminates vibrational loosening, and seals against leakage and corrosion.Typical Usessoft metal fasteners, precision screws, and locking fasteners smaller than .25.. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
|
Northstar Polymers MPN-023 Polyether Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
|
Northstar Polymers MSA-018 Isocyanate Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 1200 - 2400 cP @Temperature 25.0 °C |
1200 - 2400 cP @Temperature 77.0 °F |
Uncured |
Permabond 268 Cyanoacrylate, General purpose PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano.. |
|||
Viscosity | 1200 - 2000 cP @Temperature 25.0 °C |
1200 - 2000 cP @Temperature 77.0 °F |
Uncured |
Permabond 922 Cyanoacrylate, High temperature PERMABOND® 922 is the original allyl cyanoacrylate adhesive. It is a single part, moderate viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts. P.. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
Uncured |
Permabond LM113 Anaerobic Threadlocker Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop.. |
|||
Viscosity | 1200 - 2500 cP @Temperature 25.0 °C |
1200 - 2500 cP @Temperature 77.0 °F |
Uncured |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Viscosity | 1200 - 2500 cP | 1200 - 2500 cP | |
Huntsman Araldite LZ 8001 A-80 Brominated Resin Weight per Epoxide (EEW, g/eq) 410 to 460. Max color is 2.Comments/Applications: Bis A epoxy 80% solids in acetone (18-21% bromine). For use in manufacture of thin laminates, prepregs and rigid la.. |
|||
Viscosity | 1200 cP | 1200 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1173 B (SIBS) Linear Triblock Copolymer Description: Kraton D1173 B is a clear, linear triblock copolymer based on styrene, butadiene and isoprene with a polystyrene content of 18%. It is supplied from Brazil in the form: Kraton D1173 BT .. |
|||
Viscosity | 1200 cP @Shear Rate 100 1/s, Temperature 180 °C |
1200 cP @Shear Rate 100 1/s, Temperature 356 °F |
Melt |
Metabolix Mirelâ„¢ P4001 Sheet Extrusion Grade Bioplastic Mirelâ„¢ P4001 is a general purpose, high melt strength material suitable for cast sheet extrusion. Mirelâ„¢ P4001 is designed for a wide range of sheet applications including gift cards, prom.. |
|||
Viscosity | 1200 - 1800 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200 - 1800 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2000511D1 Platinized Carbon Ink Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working e.. |
|||
Viscosity | 1200 cP @Temperature 40.0 °C |
1200 cP @Temperature 104 °F |
|
Solvay DURAPHOS® 178 Surfactant Identification: ALKYL AMINE NEUTRALIZED ORGANIC PHOSPHATECAS: 68187-67-7Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: DURAPHOS© 178 is a concentrated amine neut.. |
|||
Viscosity | 1200 cP | 1200 cP | 1.3% NaCl added |
Solvay MACKADET® CA-ND Surfactant Product description: Mackadet CA-ND is a concentrated blend of mild surfactants for use as a base for high foaming surfactant systems. Mackadet CA-ND responds rapidly to viscosity building with the .. |
|||
Viscosity | 1200 - 1500 cP | 1200 - 1500 cP | |
Master Bond Mastersil 151 Two Component Low Viscosity Silicone Compound Master Bond MasterSil 151 is a two component, low viscosity
silicone compound for high performance potting and
encapsulation. MasterSil 151 is an addition cured system and does not require exposure.. |
|||
Viscosity | 1200 - 1500 cP @Temperature 23.0 °C |
1200 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV10MED Biocompatible One Component UV Curable Adhesive System Master Bond UV10Med is a one part UV type system for bonding, sealing and coating. It fully passes USP Class VI testing requirements and features good optical clarity and physical properties as well.. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre.. |
|||
Viscosity | 1200 cP @Temperature 25.0 °C |
1200 cP @Temperature 77.0 °F |
|
Zircar Zirconia ZR-CEM Zirconia Cement Zircar Zirconia Cement Type ZR-CEM is an off white single part yttria-stabilized zirconia adhesive with a useful temperature limit of 2200°C. ZR CEM is formulated specifically for bonding Zircar Zi.. |
|||
Viscosity | 1200 - 6000 cP | 1200 - 6000 cP | Thixotropic |
Loctite® 222MS Low Strength/Small Screw Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 1200 cP | 1200 cP | dynamic |
Dow Corning FLUOROGEL® Q3-6679 DIELECTRIC GEL KIT Two-part, clear, RT or heat cure, solvent and fuel resistant.Information provided by Dow Corning |
|||
Viscosity | 1200 - 1700 cP @Temperature 23.0 °C |
1200 - 1700 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OG142-112 UV Cure Optical Epoxy Material Description: Single component, medium viscosity, UV curable epoxy for adhesive sealing and encapsulating fiber optic and optoelectronic packaging application. Replacement version of EPO-TE.. |
|||
Viscosity | 1200 cP | 1200 cP | Nominal |
Dymax Light Weld® 426 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Viscosity | <= 1200 cP | <= 1200 cP | |
Abatron AboTar 8101-8 Solventless Tar-Epoxy Compound AboTar 8101-8 is a 2-part tar-epoxy variable-ratio system. It is weather- and water-proof, flexible, and acid, alkali, and fuel resistant. It can be used neat or with sand or aggregates. Uses: Resu.. |
|||
Viscosity | 1200 cP | 1200 cP | B Side |
ACC SMP™ EP 3001 EPI Engineered Polymers Silicone Modified Polymer EP 3001, “Powered by Reactamine® Technology”, is a two component 100% solid polyurea based sealant. EP 3001 is a self-leveling sealant designed to protect horizontal concrete. This elastomer disp.. |
|||
Viscosity | 1200 cP @Temperature 177 °C |
1200 cP @Temperature 350 °F |
Typical |
Bostik 2305 Good Heat Resistance EVA Glue Stick Bostik 2305 Good Heat Resistance EVA Glue StickGood heat resistance. Adheres to a variety of coated and uncoated board stock. |
|||
Viscosity | 1200 - 1600 cP | 1200 - 1600 cP | |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Viscosity | 1200 cP | 1200 cP | Part B |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Viscosity | 1200 - 2200 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200 - 2200 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2090130P5 Pink Dielectric Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 1200 cP @Temperature 177 °C |
1200 cP @Temperature 350 °F |
Typical |
Bostik 6305 Good Heat Resistance EVA Glue Stick Bostik 6305 Good Heat Resistance EVA Glue StickGood heat resistance. Adheres to a variety of coated and uncoated board stock. |