Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1000 - 1500 cP | 1000 - 1500 cP | |
ND Industries 331 Surface Insensitive Instant Superglue Medium-high viscosity for difficult to bond surfaces |
|||
Viscosity | 1000 cP | 1000 cP | |
Resinlab® CYNERGY CA6104 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Viscosity | 1000 cP | 1000 cP | |
Resinlab® CYNERGY CA6809 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 1000 cP | 1000 cP | Part B, RVT, #2, 2.5 rpm; TM R050-12 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Viscosity | 1000 - 2100 cP | 1000 - 2100 cP | Cement Viscosity |
Nitriflex N-5 NBR - Nitrile Rubber Excellent resistance to oils and fuel resistance with good mechanical properties. Applications: cement, adhesives, grouts, safe footwear, friction materials, safe footwear.Information provided by Da.. |
|||
Viscosity | 1000 - 13000 cP | 1000 - 13000 cP | |
Huntsman Araldite 98-311 Bisphenol F Epoxy Resin Weight per Epoxide (EEW, g/eq) 182 to 192. Max color is 2.Comments/Applications: Bisphenol A/F, modified with reactive diluents. Non-crystallizing. Very low viscosity. Used in civil engineering .. |
|||
Viscosity | 1000 - 2500 cP | 1000 - 2500 cP | |
Huntsman HY 356 Aliphatic Amine Mix Ratio with GY 6010 is 35.Comments/Applications: A medium viscosity phenol free aliphatic amine adduct. Industrial maintenance, coatings, tank lining, pipe coatings and flooring.Data provided b.. |
|||
Viscosity | 1000 cP | 1000 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1171 P (SIBS) Linear Triblock Copolymer Description: Kraton D1171 P is a clear, linear triblock copolymer based on styrene, butadiene and isoprene with a polystyrene content of 19%. It is supplied from North America in the form: Kraton D1.. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% Toluene Solution at 25°C; KM 06 |
Kraton® D1186 A (SBS) Branched Block Copolymer Description: Kraton D1186 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% Toluene Solution at 25°C; KM 06 |
Kraton® D1186 E (SBS) Branched Block Copolymer Description: Kraton D1186 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Viscosity | 1000 - 10000 cP | 1000 - 10000 cP | |
Lord Adhesives 17 Mix-In Accelerator for 200, 400, 500 Series Lord Adhesives 17 Mix-In Accelerator for 200, 400, 500 SeriesLord Accelerator 17 mix-in accelerator for Lord 200, 400 and 500 series acrylic adhesives. Use at a 10:1 ratio. |
|||
Viscosity | 1000 - 2000 cP | 1000 - 2000 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-120H TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use.. |
|||
Viscosity | <= 1000 cP | <= 1000 cP | RP-0596 |
Solvay ABEX® 18-S Surfactant Description: Proprietary surfactant systemChemical Name: Anionic SurfactantAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: ABEX© 18-S is an APE-Free anionic emuls.. |
|||
Viscosity | <= 1000 cP | <= 1000 cP | #2, 60 rpm, 1 min; RP-0596 |
Solvay REPEL-O-TEX® CRYSTAL Surfactant Description: Designed for liquid laundry formulations to impart soil release properties to polyester fabrics, offering protection against adhesion of greasy soils between wash cycles.Chemical Name: .. |
|||
Viscosity | 1000 - 4000 cP | 1000 - 4000 cP | mixed compound |
Master Bond EP38CL Adhesive Features Toughness and Durability Description: Master Bond EP38CL is a lower viscosity, optically clear two component epoxy system for high performance bonding, coating, sealing and small encapsulations, featuring toughness and dura.. |
|||
Viscosity | 1000 - 10000 cP | 1000 - 10000 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1401LG Nitrile Powder and Crumb Elastomer Nipol 1401LG is a copolymer of butadiene and acrylonitrile of excellent oil resistance. This material is ground and dusted with approximately 2.0% mineral anticake which allows direct addition to mi.. |
|||
Viscosity | 1000 cP | 1000 cP | dynamic |
Dow Corning SYL-OFF® SL 30 RELEASE MODIFIER Cost-effective; medium viscosityInformation provided by Dow Corning |
|||
Viscosity | 1000 cP | 1000 cP | |
Elmer's Products Aron Alpha® 403T Cyanoacrylate Adhesive (Industrial Krazy Glue™) Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa.. |
|||
Viscosity | 1000 - 1050 cP @Temperature 35.0 °C |
1000 - 1050 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 42 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 1000 cP | 1000 cP | "A" component |
ACC QGel 310 QSI Quantum Silicones High Strength Gel QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid.. |
|||
Viscosity | 1000 - 1700 cP | 1000 - 1700 cP | |
3M Scotch-Weld™ CA9 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting version of CA8 for wire tacking and coil terminating. Meets CID A-A-3097, Type II, C.. |
|||
Viscosity | 1000 cP | 1000 cP | |
3M Scotch-Weld™ LO1000 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Viscosity | 1000 - 2000 cP | 1000 - 2000 cP | |
Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass |
|||
Viscosity | 1000 cP | 1000 cP | Part B, RVT, #2, 20 rpm; TM R050-12 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Viscosity | 1000 cP | 1000 cP | Part A |
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru.. |