Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 10 - 25 cP | 10 - 25 cP | |
Ritelok TL90 Post Assembly Threadlocker Anaerobic. Low viscosity threadlocker for port assembly. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant |
|||
Viscosity | 10 - 25 cP | 10 - 25 cP | |
ND Industries 150 Wicking Adhesive High Pressure Sealant Seals pores in welds and hairline cracks in castings |
|||
Viscosity | 10 - 25 cP | 10 - 25 cP | |
ND Industries 150 Wicking Adhesive Sealant Threadlocker General DescriptionMedium to high strength. Locks pre-assembled fasteners through capillary action and seals porosities in welds and hairline cracks in castings.Meets military spec MIL-S-46163 Type.. |
|||
Viscosity | 10 - 30 cP @Temperature 25.0 °C |
10 - 30 cP @Temperature 77.0 °F |
Uncured |
Permabond HL126 Anaerobic Threadlocker PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi.. |
|||
Viscosity | 10 cP @Temperature 25.0 °C |
10 cP @Temperature 77.0 °F |
of Solution, 5% wt/wt in Styrene |
Polimeri Europa Europrene® SOL 1205 Styrene - Butadiene Copolymer Europrene® SOL 1205 is a solution styrene-butadiene partial block copolymer, polymerized using an alkyl lithium catalyst. A non-staining antioxidant is added during the production process.Key Feat.. |
|||
Viscosity | 10 - 30 cP | 10 - 30 cP | 0.5-10.0% solids |
Panipol Oy T Inherently Conductive Polymer Doped polyaniline in tolueneSolution Processing, Coating formulations, Ink formulationsInformation provided by Panipol Oy Ltd |
|||
Viscosity | 10 - 15 cP @Temperature 25.0 °C |
10 - 15 cP @Temperature 77.0 °F |
Uncured |
Permabond 801 Cyanoacrylate, High Temperature PERMABOND® 801 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Viscosity | 10 cP | 10 cP | D=30/s; DIN 54 453 |
3M Dyneon™ TF 5050 PTFE Dispersion
(discontinued **) Used for formulation of coating systems; impregnation.Dyneon PTFE dispersions are aqueous dispersions developed for use in metal coating formulations and for application of impregnation and fabric c.. |
|||
Viscosity | <= 10 cP | <= 10 cP | |
Lord Adhesives 26 No-Mix Accelerator for 200/500 Series Lord Adhesives 26 No-Mix Accelerator for 200/500 Series |
|||
Viscosity | <= 10 cP | <= 10 cP | |
Lord Adhesives 4 No-Mix Accelerator for 200/500 Series Lord Adhesives 4 No-Mix Accelerator for 200/500 SeriesLord Accelerator 4 is a no mix accelerator for Lord 200 and 500 series acrylic adhesives. Brush, wipe, spray or dip on one or both surfaces to b.. |
|||
Viscosity | 10 cP | 10 cP | |
Lord Adhesives 459T Toluene Adhesion Promoter for Lord Acrylic, Epoxy, Urethane and Cyanoacrylate Adhesives To meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surface modifiers. Lord® Adhesion Enhancers.. |
|||
Viscosity | 10 cP | 10 cP | |
Lord Adhesives 459X Xylene Adhesion Promoter for Lord Acrylic, Epoxy, Urethane and Cyanoacrylate Adhesives Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Viscosity | 10 cP | 10 cP | |
Lord Adhesives 7701 Ethyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Viscosity | 10 cP | 10 cP | |
Lord Adhesives 7707 n-Butyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Viscosity | 10 cP | 10 cP | B-type viscometer (60rpm) |
Mitsui UNISTOLEâ„¢ R-100K Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi.. |
|||
Viscosity | 10 cP | 10 cP | B-type viscometer (60rpm) |
Mitsui UNISTOLEâ„¢ R-100S1 Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi.. |
|||
Viscosity | 10 cP | 10 cP | |
Solvay Chemicals Rigmah® BV353 Information provided by Solvay |
|||
Viscosity | 10 cP @Temperature 25.0 °C |
10 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil OM 10 Methyl Silicone Fluid The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gi.. |
|||
Viscosity | 10 - 110 cP | 10 - 110 cP | Part B |
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin.. |
|||
Viscosity | 10 - 30 cP | 10 - 30 cP | dynamic |
Dow Corning 840 RESIN Medium-hard silicone binder resin for maintenance paints, colored baking enamels, decorative finishes. Improves heat resistance and weathering of organic resins. As an additive to improve flow-out o.. |
|||
Viscosity | 10 cP | 10 cP | |
Elmer's Products Aron Alpha® 801 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Low odor, low chlorosis (bloom) when a transparent bond, appearance and strength are required.Low gap fill. Ethoxyethyl monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. .. |
|||
Viscosity | 10 cP | 10 cP | |
Dow ISONATE™ 50 O,P` Pure MDI ISONATE™ 50 O,P` is a high ortho-para MDI designed for use in polyurethane adhesives, sealants, sports flooring, coatings, electrical encapsulants and flexible molded foams. ISONATE™ 50 O,P` offe.. |
|||
Viscosity | 10 cP | 10 cP | dynamic |
Dow Corning 1593 CLEANER/PRIMER Dow Corning 1593 Cleaner/Primer is a clear, surface cleaner that improves the adhesion of Dow Corning ® brand silicone building sealants to many porous and nonporous construction substrates. This d.. |
|||
Viscosity | 10 cP | 10 cP | 5% Styrene Solution; ASTM D445 |
Chi Mei Kibipol® PR-1205 Butadiene Rubber (SSBR) Asphalt modifier |
|||
Viscosity | 10 - 200 cP | 10 - 200 cP | |
3M Scotch-Weld™ HoldFast 70 Adhesive Extremely versatile, fast tracking industrial grade spray adhesive with unique wide-web spray pattern. Ideal for bonding a variety of substrates, including polystyrene.Features: Creates quick perman.. |
|||
Viscosity | >= 10 cP | >= 10 cP | |
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Viscosity | 10 cP | 10 cP | |
Aremco Ceramabind™ 830 High Temperature Inorganic Binder A basic solution compatible with most oxide and metal powders. Ideal for formulating high pigment-to-binder ratios to produce dense adhesives and coatings. Sets at room temperature to a moisture res.. |
|||
Viscosity | 10 - 200 cP | 10 - 200 cP | |
3M Scotch-Weld™ HoldFast 70 Cylinder Spray Adhesive Extremely versatile, fast tracking industrial grade spray adhesive with unique wide-web spray pattern. Ideal for bonding a variety of substrates, including polystyrene.Features: Creates quick perman.. |
|||
Viscosity | 10 - 20 cP @Temperature 25.0 °C |
10 - 20 cP @Temperature 77.0 °F |
Uncured |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Viscosity | 10 - 30 cP @Temperature 25.0 °C |
10 - 30 cP @Temperature 77.0 °F |
Uncured |
Permabond A126 Anaerobic Retainer Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u.. |