Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.8 cP @Temperature 25.0 °C |
1.8 cP @Temperature 77.0 °F |
|
LyondellBasell PE Propylene glycol ethyl ether Information provided by Lyondell. |
|||
Viscosity | 1.8 cP @Temperature 25.0 °C |
1.8 cP @Temperature 77.0 °F |
|
LyondellBasell Glycol Ether EBA Ethylene glycol butyl ether acetate Information provided by Lyondell. |