Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.156 cP | 1.156 cP | |
LG Chemical 2-Ethyl Hexyl Acrylate Features: Low Color- Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity -Through the multistage .. |
|||
Viscosity | 1.156 cP @Temperature 20.0 °C |
1.156 cP @Temperature 68.0 °F |
|
LG Chemical Acrylic Acid Low Inhibitor & Low Dimer - To maintain a low dimer content with small dose of inhibitor, we control storage period, storage temperature and etc. We can adjust the amount of inhibitor upon customerâ.. |