| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Index of Compound |
2.0
-
9.0
g/10 min @Temperature 190 °C |
2.0
-
9.0
g/10 min @Temperature 374 °F |
P=49, 1 H |
|
Sibur DST-45 RM Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE)
Kraton D 4271. For production of footwear compositions.
|
|||
| Melt Index of Compound |
7.0
-
9.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0
-
9.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Arkema Group LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 20 MA 08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MA 08 is a polyme..
|
|||
| Melt Index of Compound |
7.0
-
9.0
g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0
-
9.0
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Arkema Group OREVAC® 18722 Maleic Anhydride Modified Polypropylene
OREVAC 18722 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18722 ..
|
|||
| Melt Index of Compound |
7.0
-
9.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0
-
9.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4603 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure process in autoclave reactor. LOTADER 4603 is a multipurpose extrusion adhesive used..
|
|||
| Melt Index of Compound |
7.0
-
9.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0
-
9.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Arkema Group LOTRYL® 20 MBG 08 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 20MBG08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MBG 08 is a polyme..
|
|||