| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Index of Compound | 0.30 - 0.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.30 - 0.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
| Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | |
| Lushan AR-1 Nylon Toughener/PA Impact Modifier Nylon toughener/PA impact modifier Lushan series is a maleic anhydride grafted polyolefin elastomer, with a very low residual maleic anhydride monomer, no irritating odor when using. Nylon toughener.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | ASTM D1238 |
| DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman CP80-01 Linear Low-Density Polyethylene DescriptionCP 880-01 natural is a linear low-density polyethylene having good tensile, stiffness, and toughness properties.ApplicationCP 880-01 meets FDA Regulation 21 CFR 177.1250(c) 3.1 and 3.2.In.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition 190/2.16; ASTM D1238 |
| Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin Resin Type: Medium molecular weight distributionCharacteristics: Combination of toughness and tensileGood puncture resistanceMeets FDA regulations for food packaging below cooking temperaturesInform.. |
|||
| Melt Index of Compound | 0.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
| Chevron Phillips Marlex® 9514H Polyethylene; HDPE High density polyethylene. This gas phase, high molecular weight hexene copolymer is tailored for lightweight blow molded applications that: Require excellent stiffness to ESCR ratioRequire good m.. |
|||
| Melt Index of Compound | 0.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
| Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc.. |
|||
| Melt Index of Compound | 0.30 g/10 min | 0.30 g/10 min | Condition E; ASTM D1238 |
| A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||