Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 15 - 35 g/10 min | 15 - 35 g/10 min | |
Zig Sheng Industrial ZISAMIDE® TP6802 Nylon 6 ZISAMIDE® TP6802 is a Polyamide 6. Application: compounding extrusionInformation provided by ZIG SHEN Industrial Co., LTD. |
|||
Melt Index of Compound | 25 - 35 g/10 min @Load 2.16 kg, Temperature 190 °C |
25 - 35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |