Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 43 g/10 min @Load 2.16 kg, Temperature 330 °C |
43 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. |
|||
Melt Index of Compound | 43 g/10 min @Load 1.20 kg, Temperature 300 °C |
43 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Melt Index of Compound | 43 g/10 min @Load 1.20 kg, Temperature 300 °C |
43 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Melt Index of Compound | 43 g/10 min @Load 1.20 kg, Temperature 300 °C |
43 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Melt Index of Compound | 43 g/10 min @Load 2.16 kg, Temperature 330 °C |
43 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Index of Compound | 43 g/10 min @Load 2.16 kg, Temperature 330 °C |
43 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Index of Compound | 43 g/10 min @Load 2.16 kg, Temperature 330 °C |
43 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Index of Compound | 43 g/10 min @Load 2.16 kg, Temperature 330 °C |
43 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Melt Index of Compound | 43 g/10 min @Load 2.16 kg, Temperature 330 °C |
43 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Melt Index of Compound | 43 g/10 min @Load 2.16 kg, Temperature 330 °C |
43 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Melt Index of Compound | 43 g/10 min @Load 1.20 kg, Temperature 300 °C |
43 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Melt Index of Compound | 43 g/10 min @Load 2.16 kg, Temperature 330 °C |
43 g/10 min @Load 4.76 lb, Temperature 626 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |