Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE EC88R Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T3020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF3045 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF3050 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC GF3020 PB7 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC K3020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH T3022D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polykemi AB POLYform POM C M20 AS4 Polyoxymethylene, Antistatic Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 372 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ PFA 6503 C EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 C EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 155-1339 LMDPE Rotational Molding Resin Description: ICORENE 155-1339 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Melt Index of Compound | 3.0 g/10 min @Temperature 230 °C |
3.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Mitsui ADMER® QF500A PP Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 3.0 g/10 min @Temperature 190 °C |
3.0 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® NF498A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Europe-Africa-Middle East) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East) PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)... |
|||
Melt Index of Compound | 3.0 g/10 min @Temperature 230 °C |
3.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P90BD Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8450 Polyolefin Elastomer Description: Engage® 8450 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 21.6 kg, Temperature 150 °C |
3.0 g/10 min @Load 47.6 lb, Temperature 302 °F |
Fainplast |
Fainplast Compounds HAX HF 4522 Halogen Free PVC High flame retardancy |
|||
Melt Index of Compound | 3.0 g/10 min @Load 21.6 kg, Temperature 150 °C |
3.0 g/10 min @Load 47.6 lb, Temperature 302 °F |
|
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 372 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ FEP 6303Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6303Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTADER® TX 8030 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER TX 8030 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER TX 8030 is an adhesive designed for extrusion coating .. |
|||
Melt Index of Compound | 3.0 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group EVATANE® 28-03 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-03 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melt Index of Compound | 3.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PP TOUCH 34725 Polypropylene, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH TS3020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 3.0 g/10 min | 3.0 g/10 min | |
Lushan OR-1 Halogen-Free Flame-Retardant Compatibilizer Halogen-free flame retardant compatibilizer Lushan series for cables and wires are developed by several doctors and maters from Lushan’s R&D Center, and combined ten years’ modified polyolefin gra.. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 5.00 kg, Temperature 372 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ PFA 6503 B EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 B EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |
|||
Melt Index of Compound | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical HI835M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |